Sign In | Join Free | My adobecards.com
adobecards.com
Products
Search by Category
Home > Magnetic Materials >

Waspaloy, 2.4654, N07001, Nickel Alloy Spring Wire

Categories Nickel Spring Wire
Brand Name: fushun
Model Number: 2.4654
Certification: ISO NQA
Place of Origin: CHINA
MOQ: 1KG
Payment Terms: L/C, T/T, D/P, D/A
Delivery Time: 1
Material: Nickel Alloy
Application: Spring
  • Haven't found right suppliers
  • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
  • And this service is free of charge.
  • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
Submit Buying Request
  • Product Details
  • Company Profile

Waspaloy, 2.4654, N07001, Nickel Alloy Spring Wire

Waspaloy, 2.4654, N07001, Nickel Alloy Spring Wire

This age hardenable nickel base super alloy has very good strength in temperatures up to about 980°C (1800°F). It’s strength is generally comparable to that of Rene 41 and is generally superior to that of Alloy 718 at temperatures exceeding 650 – 705°C (1200 – 1300°F).


Size

Diameter: 0.1 - 40mm

Shape: round, square, flat, special shaped


Key Features

  • Very high strength at elevated temperatures.
  • Strength is generally comparable to that of Rene 41 and generally superior to Inconel 718.
  • Age hardenable.
  • High temperature dynamic applications.

Typical Applications

Gas turbine engine parts

Aerospace components

Springs and fasteners


Designations

W.Nr 2.4654

UNS N07001

AWS 170


Specifications

AMS 5544

AMS 5706

AMS 5708

AMS 5828

ASTM B637


Chemical Composition

ElementMin %Max %
C0.020.1
Mn0.1
Si0.1
P0.01
S0.01
Cr1821
Co1215
Mo3.55
Ti2.753.5
Al1.21.6
B0.0030.01
Zr0.04
Fe2
Cu0.1
Nibalbal

Physical Properties

DensityMelting PointCoefficient of ExpansionModulus of RigidityModulus of Elasticity
8.16 g/cm³1330 °C12.2 μm/m °C (20 – 100 °C)81 kN/mm²211.0 kN/mm²
0.295 lb/in³2425 °F6.8 x 10-6 in/in °F (70 – 212 °F)11750 ksi30600 ksi

Heat treatment

ConditionTypeTemperatureTimeCooling
AnnealedStabilize
Age Harden
843 °C (1550 °F)
760 °C (1400 °F)
4 Hr
16 Hr
Air
Air
Spring TemperAnneal
Stabilize
Age Harden
1050 °C (1920 °F)
843 °C (1550 °F)
760 °C (1400 °F)
4 Hr
4 Hr
16 Hr
Air
Air
Air

Mechanical Properties

Solution AnnealedApprox. tensile strength<1100 N/mm²<159 ksi
Approx. operating temperature depending on load and environment
Solution Annealed + AgedApprox. tensile strength1300 – 1500 N/mm²189 – 218 ksi
Approx. operating temperature depending on load and environmentup to +550 °Cup to +1020 °F
Spring TemperApprox. tensile strength1300 – 1600 N/mm²189 – 232 ksi
Approx. operating temperature depending on load and environment
Spring Temper + Annealed + AgedApprox. tensile strength1300 – 1500 N/mm²189 – 218 ksi
Approx. operating temperature depending on load and environmentup to +550 °Cup to +1020 °F

Quality Waspaloy, 2.4654, N07001, Nickel Alloy Spring Wire for sale
Send your message to this supplier
 
*From:
*To: Hunan Fushun Metal Co., Ltd.
*Subject:
*Message:
Characters Remaining: (0/3000)
 
Inquiry Cart 0