Name: | Stainless Steel Sign Letters |
Colors: | Blue, green, silver, darkgray, client's requests |
Surface treatments: | Brushed, mirror,sandblast,random pattern,snow sand, embossed pattern Applications Hospital, Office building, Residential House, Exhibition Center,Schools, Restaurants, Commercial Buildings |
Guarantee: | 20 years |
Applications: | Road beside Hospital, Office building, Residential House, Exhibition Center,Schools, Restaurants, Commercial Buildings |
Materials: | 201/304/316 |
Company Info. |
String One Technology Co.,Ltd. |
View Contact Details |
Product List |
Custom Stainless Steel Signs With Designed Patterns For Company Sign
Stainless steel sign features
Stainless steel sign
Stainless steel sign making process
Ferric chloride corrosion stainless steel sign
a. The effect of concentration. Chemical Corrosion We also call the
micro-battery corrosion, the more positive the redox potential, the
faster the corrosion rate. As the concentration increases, the
redox potential becomes positive and the corrosion rate increases.
Industrial grade ferric chloride is not high in purity, and its
redox potential is relatively negative. Only when the Baume degree
reaches 42 or higher, the redox potential can meet the requirements
of corrosion of stainless steel.
b. Effect of pH on the corrosion rate in solution. The PH value is
low, which is strong against the corrosion of stainless steel; the
pH value is too high, and the ferric chloride is hydrolyzed into
iron hydroxide precipitate, which loses the corrosion effect. The
pH of the corrosive liquid used in production should be adjusted to
a certain extent.
c. Effect of the temperature of the corrosive solution. The higher
the temperature of the corrosive liquid, the faster the corrosion
rate. However, considering the resistance of the
corrosion-resistant ink, the temperature should be controlled
between 30--40 °C.